When to use "hot" mud This allows the pros to tape and first coat seams all within the first day on a job. Many pros feel that quick-setting mud provides a stronger base coat and therefore protects better against cracking.
Full Answer
How to use hot mud safely?
As with any chemical substance, follow the instructions on the package precisely and adhere to any rules of safe usage. You should begin by filling your mixture bucket with water; if you put the powder in first, the texture of your hot mud won’t be right.
Why is it called hot mud?
As the mud hardens, the chemical reaction creates a small amount of heat which may be a reason some people call it hot mud. On the other hand it could be just an idiomatic description emphasizing that you have to move quickly once mixed because it will harden up on you if you don't finish within its specified time. What is Durabond ®?
Is hot mud or cement better for drywall?
Plus, hot mud tends to be cheaper, since the burden of the labor rests on the purchaser. Hot mud drywall products tend to act like cement once they’re mixed in that they have a limited lifespan before they harden beyond usability. However, the hot mud drywall compound gives you a tough bond and sturdy result.
Should I use joint compound or hot mud?
Typically when you can tape and coat a project and then come back the next day normal joint compound is the most efficient to use because of the lack of a need to mix it. There are however applications where hot mud is the “miracle” product. When I’m doing repairs I use 5 minute hot mud exclusively.
Is hot mud better?
5:246:53Hot mud basics - Drywall Instruction - YouTubeYouTubeStart of suggested clipEnd of suggested clipIt takes a long time to dry and then it also shrinks down and so hot mud is great for pre filling.MoreIt takes a long time to dry and then it also shrinks down and so hot mud is great for pre filling.
When should you use hot mud?
When to use "hot" mud. Quick-setting drywall mud is great for small patch jobs where you don't want to wait 24 hours before applying a second coat. Hot mud is also used on large drywall jobs for bedding-in mesh drywall tape. This allows the pros to tape and first coat seams all within the first day on a job.
Can hot mud be used for all coats?
Topping mud has less adhesion properties than all-purpose mud, so it's not suitable for first and second coats. Lightweight all-purpose mud also dries to a lighter shade, making it suitable for walls that will take pale paint.
How thick can you apply hot mud?
The average thickness of Sheetrock mud is about a quarter of an inch (0.64 cm). However, you can apply it up to a thickness of 12 centimeters (4.72 in). It would be best to keep it flush with your walls, so the thickness may vary depending on the spot.
Can you skim coat with hot mud?
0:070:43DO NOT Skim Coat with Hot Mud! - YouTubeYouTubeStart of suggested clipEnd of suggested clipYou are not supposed to skim coat with a hot mud it will fail or it might not even dry let's take aMoreYou are not supposed to skim coat with a hot mud it will fail or it might not even dry let's take a look at the back of the bag of this sheetrock.
Is hot mud the same as joint compound?
Commonly called "hot mud," quick-setting compound is ideal when you need to finish a job quickly or when you want to apply multiple coats on the same day. Sometimes called simply "setting compound," this form is also useful for filling deep cracks and holes in drywall and plaster, where drying time can become an issue.
How long before you can paint over hot mud?
Hot mud is a powder that you mix with water. It is formulated to set like plaster, so it dries in just 20 to 60 minutes. You can choose from products that have a faster or slower drying time. One downside is that the rapid dry time does not allow much time to fix errors.
Is two coats of mud enough?
If your wall has distinct crevices, cracks, or textured areas, or if your brand of drywall mud isn't offering enough coverage, you may have to do a couple of additional coats of compound. However, in general, you'll need one coat to fill in the seams and three more coats after taping.
Will drywall mud crack if too thick?
The most common cause of cracking in freshly applied drywall mud is when it is applied too thickly. This exacerbates the issue with evaporation-based drying and can even crack curing compounds. Past this point, applying more drywall mud will cause the cracking to worsen if done improperly.
What happens if drywall mud is too thick?
Any drywall joint can also crack if the mud is applied too thick or too quickly. To prevent cracking, don't use more mud than you need for any of the coats, and let each coat dry completely before adding the next.
Should drywall joints be tight?
Hanging Drywall Vertically: Leave a 1/8-in. It'll usually just cause trouble. Jamming in a piece that's too tight will crumble the edge or break out a corner (left). And removing a piece to shave a too-tight edge is messy and time consuming. A loose fit avoids this problem.
How does hot mud harden?
When it comes to hot-mud, there is a difference between hardening and drying. Hot mud hardens by means of a chemical reaction. Manufacturers mix different amounts of hardening agents into the material causing it to set up at different times. Hot mud is packaged according to the time it takes to harden.
What is hot mud?
The plastic lining keeps moisture out and preserves freshness. Keeping the powdered mud dry is critical. When water comes in contact with hot mud it begins an irreversible chemical reaction that causes the mud to harden.
What is drywall mud used for?
It is sometimes used to first coat seams and corner beads.
What is Durabond mud?
Durabond ® is a trademarked name that refers specifically to a product made by USG ®. It was one of the first types of quick setting drywall mud that was used extensively in the workplace and for this reason the name became ubiquitous with quick setting drywall mud.
How many gallons of drywall mud is in a box?
Most often, the boxes of mud are also 4.5 gallons in volume but occasionally you will find 3.5 gallon boxes.
What is pre-mixed drywall mud?
Pre-mixed drywall mud is, as the name indicates, pre-mixed and ready to use. Pre-mixed drywall mud is almost always thinned with water before using. The amount of water used depends on how the mud will be applied. For example, bedding in tape requires a thinner than normal consistency.
How long does it take for hot mud to set?
Actual working time is generally less than the time listed. For example, 45-minute hot mud may begin to set up in 30-35 minutes. The working time can vary slightly depending on a few factors. High humidity or cooler temperatures causes hot mud to take longer to set.
Garage Drywall: Hot Mud vs. Premixed Joint Compound
I have started to tackle the garage makeover, and the very first thing I needed to do was repair the unfinished drywall. Because there is so much junk in the garage, I decided I would tackle it wall-by-wall.
Share this
I recently removed Disqus comments and converted to the Facebook commenting system.